Plât Titaniwm Gr1

Plât Titaniwm Gr1

Taflen titaniwm CP
UNS R50250 3.7025
BT1-00
Anfon ymchwiliad
Sgwrs Nawr
Disgrifiad

 

Cyflwyniad Cynhyrchion

1. Plât Titaniwm Gr1yw'r titaniwm pur fasnachol puraf, mae ganddo berfformiad ffurfio a gwrthsefyll cyrydiad da.

2. Gwybodaeth Sylfaenol

Manylebau

Gradd: Gr1, BT1-00, BT1-0, ac ati.

Safonau: ASTM B265, AMS4911, AMS4911H, GB/T3621-2007

Maint: T x W x L (mm)Proses
T (4.1-60.0) x W (400-3000) x L (1000-4000) Rholio Poeth
T (0.3-4.0) x W (400-1500) x L (1000-3000) Rholio oer

Sioeau Manylion


thin titanium sheet

Taflen titaniwm CP

Titanium sheet metal

dalen fetel titaniwm

3. Priodweddau Titaniwm

Mae gan ditaniwm ymwrthedd cyrydiad rhagorol, priodweddau mecanyddol, a phriodweddau prosesau, ac fe'i defnyddir yn helaeth mewn llawer o sectorau o'r economi genedlaethol. Yn enwedig mewn cynhyrchu cemegol, defnyddir titaniwm i ddisodli dur di-staen, aloion sy'n seiliedig ar nicel, a metelau prin eraill fel deunyddiau sy'n gwrthsefyll cyrydiad. Mae hyn o arwyddocâd mawr i gynyddu allbwn, gwella ansawdd y cynnyrch, ymestyn oes offer, lleihau'r defnydd, lleihau'r defnydd o ynni, lleihau costau, atal llygredd, gwella amodau llafur, a gwella cynhyrchiant llafur.

4. Beth yw cyfansoddiad cemegolTi plât Gr1 Gr2 a Gr5?


N

C

H

Fe

O

Al

V

Pa

Mo

Ni

Ti

Gr 1

0.03

0.08

0.015

0.20

0.18

/

/

/

/

/

bal

Gr 2

0.03

0.08

0.015

0.30

0.25

/

/

/

/

/

bal

Gr 5

0.05

0.08

0.015

0.40

0.20

5.5~6.75

3.5~4.5

/

/

/

bal

5. eiddo tynnol plât metel titaniwm:

Gradd

Tynnol

cryfder (munud)

Cnwd

cryfder (munud)
elongation ( cant )

Ksi

MPa

Ksi

MPa

1

35

240

20

138

24

2

50

345

40

275

20

5

130

895

120

828

10

6. Ceisiadau Plât Titaniwm:

Defnyddir plât titaniwm Gr1 yn bennaf ar gyfer stampio rhannau a rhannau strwythurol sy'n gwrthsefyll cyrydiad gyda thymheredd gweithio o dan 360 gradd, megis tiwb sy'n gwrthsefyll cyrydiad morol, falf, pwmp, cydrannau system dihalwyno, a chemegol. cyfnewidwyr gwres. Fe'i defnyddir yn eang mewn cyfnewidwyr gwres, cemegol, meddygol ac awyrofod. offer diwydiannol.

7. Gr1 titaniwm rhestr stoc plât

GraddSpecArwynebsafonau
Gr10.4*1008*Cwyneb llacharASTMB265
Gr10.5*1000*Cwyneb llacharASTMB265
Gr10.5*1000*Cwyneb llacharASTMB265
Gr10.5*1190*Cwyneb llacharASTMB265
Gr10.5*1200*Cwyneb llacharASTMB265
Gr10.5*1220*Cwyneb llacharASTMB265
Gr10.6*1030*Cwyneb llacharASTMB265
Gr10.8*1007*Cwyneb llacharASTMB265
Gr11.0*1000*Cwyneb llacharASTMB265
Gr11.0*1000*Cwyneb llacharASTMB265
Gr11.0*1000*Cwyneb llacharASTMB265
Gr11.0*1007*Cwyneb llacharASTMB265
Gr11.0*1180*Cwyneb llacharASTMB265
Gr11.0*1250*Cwyneb llacharASTMB265
Gr11.0*1250*Cwyneb llacharASTMB265
Gr11.2*1046*Cwyneb llacharASTMB265
Gr11.2*1220*Cwyneb llacharASTMB265
Gr11.2*1220*Cwyneb llacharASTMB265
Gr11.2*1228*Cwyneb llacharASTMB265
Gr11.2*1505*Cwyneb llacharASTMB265
Gr11.4*1250*Cwyneb llacharASTMB265
Gr11.5*1000*Cwyneb llacharASTMB265
Gr11.5*1000*Cwyneb llacharASTMB265
Gr11.5*1000*Cwyneb llacharASTMB265
Gr11.5*1010*Cwyneb llacharASTMB265
Gr11.5*1250*Cwyneb llacharASTMB265
Gr11.5*1250*Cwyneb llacharASTMB265
Gr11.5*1250*Cwyneb llacharASTMB265
Gr11.5*1305*Cwyneb llacharASTMB265
Gr11.5*1500*Cwyneb llacharASTMB265
Gr12.0*1000*Cwyneb llacharASTMB265
Gr12.0*1000*Cwyneb llacharASTMB265
Gr12.0*1016*Cwyneb llacharASTMB265
Gr12.0*1210*Cwyneb llacharASTMB265
Gr12.0*1200*Cwyneb llacharASTMB265
Gr12.0*1220*Cwyneb llacharASTMB265
Gr12.0*1220*Cwyneb llacharASTMB265
Gr12.0*1220*Cwyneb llacharASTMB265
Gr12.0*1226*Cwyneb llacharASTMB265
Gr12.0*1227*Cwyneb llacharASTMB265
Gr12.0*1250*Cwyneb llacharASTMB265
Gr12.0*1250*Cwyneb llacharASTMB265
Gr12.0*1250*Cwyneb llacharASTMB265
Gr12.0*1250*Cwyneb llacharASTMB265
Gr12.0*1250*Cwyneb llacharASTMB265
Gr12.0*1235*Cwyneb llacharASTMB265
Gr12.0*1260*Cwyneb llacharASTMB265
Gr12.0*1505*Cwyneb llacharASTMB265
Gr12.5*1000*Cwyneb llacharASTMB265
Gr12.5*1000*Cwyneb llacharASTMB265
Gr12.5*1000*Cwyneb llacharASTMB265
Gr12.5*1500*Cwyneb llacharASTMB265
Gr13.0*1000*Cwyneb llacharASTMB265
Gr13.0*1000*CpicloASTMB265
Gr13.0*1005*Cwyneb llacharASTMB265
Gr13.0*1020*Cwyneb llacharASTMB265
Gr13.0*1020*CpicloASTMB265
Gr13.0*1200*CpicloASTMB265
Gr13.0*1220*CpicloASTMB265
Gr13.0*1220*CpicloASTMB265
Gr13.0*1220*Cwyneb llacharASTMB265
Gr13.0*1220*CpicloASTMB265
Gr13.0*1220*CpicloASTMB265
Gr13.0*1220*CpicloASTMB265
Gr13.0*1510*Cwyneb llacharASTMB265
Gr14.0*1000*CpicloASTMB265
Gr14.0*1010*CpicloASTMB265
Gr14.0*1230*CpicloASTMB265
Gr14.0*1230*CpicloASTMB265
Gr14.0*1500*CpicloASTMB265
Gr15.0*1010*CpicloASTMB265
Gr16.0*1007*CpicloASTMB265
Gr16.0*1035*CpicloASTMB265
Gr16.0*1500*CpicloASTMB265

8. Pam dewis ni?

Ardystiad: ISO 9001: 2008

Isafswm Archeb Nifer / Pwysau: 1 pc

Maes gwasanaeth: Asia, Gogledd America, De America, Ewrop, Affrica ac Ynysoedd y De.

Amser dosbarthu: 7 ~ 9 diwrnod trwy gyflym, 3 ~ 5 diwrnod mewn awyren, ar y môr yn ôl cyrchfannau.

Ffoniwch ni nawr i brynu plât titaniwm gr1, cael y pris plât ti neu anfon e-bost atom i gael y pris taflen titaniwm fesul kg, byddwn yn falch o siarad am eich ymholiad.

Tagiau poblogaidd: plât titaniwm gr1, cyflenwyr, gweithgynhyrchwyr, ffatri, pris, swmp, ar werth, mewn stoc, prynu disgownt

Anfon ymchwiliad

(0/10)

clearall