ASTM B265Strip, Taflen, a Phlât
ASTM B338Tiwbiau Wedi'u Weldio'n Ddi-dor
ASTM B348Bar a Billet
ASTM B363Ffitiadau
ASTM B367Cestyll
ASTM B381Forgings
ASTM B861Pibell Ddi-dor
ASTM B862Pibell wedi'i Weldio
ASTM F67Titaniwm Unalloyed ar gyfer Mewnblaniadau Llawfeddygol
AWS A5.16WeldIo Wire
ISO 5832-2Titaniwm Unalloyed ar gyfer Mewnblaniadau Llawfeddygol